Acid Proofing / Acid Proof Bricks

Anti-static Acid Proof Bricks

Anti-static is a grade in Shanker Agencies’ acid proof bricks range.

Anti-static grade acid proof bricks supplied by Shanker Agencies
Grade
Anti-static
Cold crushing strength
45 MPa

Anti-static technical specification

Typical values for Anti-static acid proof bricks. Test methods vary by property and product family, so confirm the applicable standard against the manufacturer datasheet before specifying.

Water absorption
<2%
Acid resistance
99% min
Alkali resistance
85%
Cold crushing strength
45 MPa
Size
230×113×65mm std

Where Anti-static is used

Acid storage tank lining (H₂SO₄, HNO₃, HCl, H₃PO₄)Reaction vessel and reactor liningAbsorption tower internal liningChimney and flue gas duct liningEffluent treatment plant sumps and channelsFertiliser plant, sulphuric acid plantPickling tank lining (steel processing)Battery room floors
Compare Anti-static with other grades▾

Compare Anti-static against every grade SAPL stocks in this family.

Swipe to compare grades

GradeWater absorptionAcid resistanceAlkali resistanceCold crushing strengthSize
Class I3-6%97% min75%40 MPa230×113×65mm std
Class II<2%99% min85%50 MPa230×113×65mm std
Class III<0.5%99.5% min90%55 MPaCustom
Carbon-Fill<1%99.5% min95%45 MPaStandard + custom
Anti-staticthis grade<2%99% min85%45 MPa230×113×65mm std

Send the drawing, dimensions, application and quantity for Anti-static acid proof bricks. Our technical team reviews the requirement and advises on grade and fulfilment route.

Request Anti-static Quote

Installation notes

  1. 1Surface preparation: concrete or steel substrate must be clean, dry, and free of oil/grease
  2. 2Apply primer coat, epoxy primer for steel, concrete primer for concrete substrate
  3. 3Use appropriate acid-resistant cement: furan resin (best acid resistance), phenolic resin, or potassium silicate
  4. 4Bed mortar thickness: 3–6 mm, applied to both brick and substrate (buttered joint)
  5. 5Joint width: 3–6 mm, fully filled with acid-resistant mortar
  6. 6Curing: furan resin mortars, 24 hrs at 25°C before any chemical exposure; heat curing improves performance
  7. 7Test before commissioning: hydraulic leak test or chemical spot test

Disclaimer: values are typical and compiled by Shanker Agencies Pvt. Ltd. from standard industry data and published manufacturer specifications. They are indicative, not a guarantee. Confirm the exact grade datasheet before specifying. For a certified datasheet or quotation, contact info@shankeragencies.com or +91 98999 57888.